All times are UTC + 2 hours




Post new topic Reply to topic  [ 3 posts ] 
Author Message
 Post subject: Dish Head Inspection
PostPosted: Thu Jan 29, 2009 7:38 am 
Offline

Joined: Fri Dec 19, 2008 3:21 am
Posts: 9
The two pcs plate of top dish head are welded.The longitudinal seam is required to inspection before forming.Is there any procedure to RT or Dye-Pent to the longitudinal seam before forming?Tq


Top
 Profile  
 
 Post subject: Re: Dish Head Inspection
PostPosted: Fri Jan 30, 2009 1:46 pm 
Offline
----------------
----------------

Joined: Thu Aug 21, 2008 9:08 am
Posts: 34
When dish end blanks has lon seam then RT ( provided joint efficiency is 1) is always taken after forming.
You also need to follow offset tolerance as specified in UW 33. There is no harm to conduct RT before forming if cost allows you to do so. RT before forming will not nullify requirement after forming but will help you to attaend defects if any. refer your Inspectio and Test Plan for requirements such as Dye Penetrant test. Section VIII Div 1 never ask this test.

[quote="akim"]The two pcs plate of top dish head are welded.The longitudinal seam is required to inspection before forming.Is there any procedure to RT or Dye-Pent to the longitudinal seam before forming?Tq[/quote]

"RT ( provided joint efficiency is 1) is always taken after forming".
Where does it come from? can you quote the paragraph?

"Section VIII Div 1 never ask this test"
Read UHA-34, UW-13, UW-50 & UW-34,(see for Note 7, page136, for both para.), UW-42. And others, may be.

Mauro


Top
 Profile  
 
 Post subject: Re: Dish Head Inspection
PostPosted: Sun Feb 01, 2009 7:44 am 
Offline
----------------
----------------

Joined: Thu Dec 11, 2008 7:55 am
Posts: 47
Location: Oregon
Per UW-2 and UW-11, full RT of butt joints is required for lethal vessels, for unfired steam boilers, and for other vessels depending on the material thickness and material class per Subsection C of Section VIII-1.
The second question is, is it a hot forming process or a cold forming? Per UHA-33, in some instances you need to do RT after hot forming.
So, you need to provide more information, including why RT is required.

Thanks,

_________________
AI-OR-US


Top
 Profile  
 
Display posts from previous:  Sort by  
Post new topic Reply to topic  [ 3 posts ] 

All times are UTC + 2 hours


Who is online

Users browsing this forum: No registered users and 0 guests


You cannot post new topics in this forum
You cannot reply to topics in this forum
You cannot edit your posts in this forum